FERRITT EPC KJERNER

FERRITT EPC KJERNER

product-351-290

 

MODELL

G.W

STØRRELSE (mm)

A

Bmin

C

D

E

F

G

Hmin

EPC13

2.5

13.3±0.3

8.3

5.6±0.2

4.6±0.2

4.5±0.2

6.6±0.2

2.1±0.1

10.5

EPC17.8

5.6

17.8±0.4

11.5

7.4±0.2

6.0±0.2

6.0±0.2

8.7±0.2

2.8±0.1

14.3

EPC34

62

34.0±0.5

19.7

14.5±0.2

14.5±0.2

16.4±0.2

20.9±0.2

9.1±0.2

24.8

EPC39

78

39.0±0.7

24.7

17.6±0.3

15.5±0.2

14.1±0.3

19.6±0.2

9.7±0.1

30.5

EPC41

108

41.0±0.6

23.6

18.5±0.2

16.5±0.2

18.9±0.2

24.5±0.2

11.0±0.2

28.8

 

MODELL

PARAMETER

AL±25 %(nH/N^2)

N.W(g)

C1mm-1

Lemm

Aemm2

Vemm3

ZP40

EPC13

2.46

30.6

12.5

382.0

870

2.1

EPC17.8

1.77

40.2

22.7

917.0

1200

4.5

EPC34

0.73

89.6

122.6

10985.0

3200

56.0

EPC39

0.60

87.95

147.0

12960.0

3700

70.5

EPC41

0.57

104.1

183.2

19064.0

4100

97.0

Populære tags: ferritt epc kjerner, Kina ferritt epc kjerner produsenter, leverandører, fabrikk